GLASS
Heat-treated glass with larger breakage fragments than tempered glass; laminate where fragment retention is required.
Request a quote| Strength vs annealed | Approx. 2× |
|---|---|
| Surface compressive stress | 24–69 MPa |
| Thermal difference stated | Approx. 75–100°C |
| Product standard | GB/T 17841-2008 |